• Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
  • Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
  • Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
  • Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
  • Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
  • Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S

Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S

Molecular Principal Chain: Element Organic Polymer
Color: Pink Turbid
Appearance: Pink Turbid
Viscosity 25 Degree PA.S: 350 - 450cps
Gel Time 25 Degree Min: 25-35min
Solid Content: 37.5 - 41.5%
Samples:
US$ 2/kg 1 kg(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2013

Suppliers with verified business licenses

Jiangsu, China
to see all verified strength labels (12)
  • Overview
  • Product Description
  • Technical Data Sheet
  • Packing Photos
  • Application photos
Overview

Basic Info.

Model NO.
2504PT-S
Thixotropic Index
1.0 - 2.0
Acid Value
17 - 27 Mg KOH/G
Transport Package
Drum
Specification
A Grade Quality
Trademark
ETERSET
Origin
China
HS Code
39079100
Production Capacity
10000ton/Year

Product Description

Product Description
 
ETERSET 2504PT-S is a thixotropic, prepromoted resilient polyester containing no wax.
It uesed for general purpose hand lay-up of small parts.

Features:
Offers high impact strength.
Provides medium-fast cure.
Gives good wet-out.
Has good strength in laminates.
Has medium thixotropic index.

 
Technical Data Sheet
Item Test result
Appearance Pink turbid
Styrene content, % 37.5 - 41.5
Viscosity , cps
( Brookfield spindle#3, 60rpm, at 25ºC)
350 - 450
Thixotropic index
( Brookfield spindle#3, 6/60rpm, at 25ºC)
1.0 - 2.0
Acid value, mg KOH/g  17 - 27

Typical Curing Characteristics:
Item Test result
Gel time, mins. 25-35
Total time to peak exotherm, mins. 40-70
Peak exotherm temperature, ºC ≥110
Note: Room temperature cure at 25ºC, 1.0% MEKPO (55%)

Typical Physical Properties:
Clear casting, ETERSET 2504PT-S
Item Test result
Barcol (934- 1) hardness 41
Tensile strength, kgf/mm2
(ASTM D 638)
6.0
Elongation, %
(ASTM D 638)
2.3
Flexural strength,kgf/mm2
(ASTM D 790)
11
Flexural modulus,kgf/mm2
(ASTM D 790)
300
Heat deflection temperature, ºC 67

Glass Fiber Laminates (450g/m2 3 layers)
Item Test result
Tensile strength, kgf/mm2 (ASTM D 638) 11.6
Flexural strength,kgf/mm2 (ASTM D 790) 17.6
Flexural modulus,kgf/mm2 (ASTM D 790) 730
Fiber content, % 30
Packing Photos

Standard packing is 200 kg steel drum.

Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
Application photos
Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S
Resilient Polyester Resin for Hand Lay-up Eterset 2504PT-S

Give us a chance, and we' ll return you with satisfaction. 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now